What should I do if there are two colors occurred in the plastic electroplating gun color?

home appliane housing chrome plating

How to solve the two-color problem of plastic electroplating gun color?

  1. The longer the product is placed after the primer, the easier it is to produce chromatic aberration. The electroplated finished product is not sprayed with topcoat for a long time, which will also cause this problem.
  2. Electric current and voltage, rotation, evaporation time, amount, and placement of electroplating materials will all have an impact, as will the degree of vacuum.
  3. The air humidity in the electroplating workshop will affect the color difference, as will the size and shape of the workpiece. 4. The primer is not dry, which is also an important reason for the color difference.
  4. The purity of the electroplating material will also lead to a chromatic aberration on the surface of the electroplated parts. In order to ensure the color quality of electroplating parts, manufacturers need to confirm the standard color sample and a color difference reference sample of electroplating parts with customers before mass production, so as to help electroplating factories to refer to proofing.